Fracture resistance of monolithic gradient zirconia crowns with different finish line designs and cement spaces
2024

Fracture Resistance of Zirconia Crowns

Sample size: 60 publication Evidence: high

Author Information

Author(s): AbdElaziz Mohammed H., Aldamaty Mohamed F., Omar Elsayed Ali, Elbadawy Adel A., Borzangy Sary, Alqutaibi Ahmed Y., Zafar Muhammad S.

Primary Institution: Taibah University

Hypothesis

The study aimed to assess how various finish line designs and cement space thicknesses affect the fracture resistance of YML zirconia crowns.

Conclusion

Knife-edge margins with YML gradient zirconia crowns provide a reliable alternative to shoulder margins, particularly in minimally invasive preparations.

Supporting Evidence

  • The rounded shoulder pattern exhibited significantly higher failure load values.
  • No significant differences between chamfer and knife-edge patterns were observed.
  • A cement space of 80 μm is preferred for various finish line designs.

Takeaway

This study looked at how different designs of dental crowns affect their strength. It found that a certain type of edge is just as good as a more traditional one, and a thicker layer of cement is better.

Methodology

Sixty crowns were fabricated and categorized into three groups based on finish line type and further divided by cement space thickness, then tested for fracture resistance.

Limitations

The use of metal dies instead of natural teeth may limit the applicability of the findings to real-world dental scenarios.

Statistical Information

P-Value

p=0.000

Statistical Significance

p<0.05

Digital Object Identifier (DOI)

10.1016/j.jtumed.2024.11.008