Fracture resistance and failure mode of three esthetic CAD-CAM post and core restorations
2024

Fracture Resistance of Three Aesthetic CAD-CAM Post and Core Restorations

Sample size: 39 publication Evidence: high

Author Information

Author(s): Fathey Islam, Azer Amir Shoukry, Abdelraheem Islam M.

Primary Institution: Faculty of Dentistry, Alexandria University

Hypothesis

No difference would be observed in fracture resistance among three non-metallic esthetic post and core restorations.

Conclusion

Both FRC and PICN demonstrated good performance regarding fracture resistance, surpassing that of PEEK.

Supporting Evidence

  • Custom PEEK post and core restorations displayed the least fracture load values at 286.16 ± 67.09 N.
  • FRC exhibited the highest average fracture load at 452.60 ± 105.90 N.
  • 46.2% of specimens with PICN were deemed non-restorable.

Takeaway

This study tested three types of dental materials used for tooth restorations to see which one is the strongest, and found that two of them are better than the third.

Methodology

Thirty-nine single-rooted human maxillary central incisors were treated and restored with three different materials, then tested for fracture resistance.

Limitations

The study could not fully replicate in vivo conditions and did not include crown restoration.

Participant Demographics

Thirty-nine human maxillary central incisors extracted due to periodontal reasons.

Statistical Information

P-Value

<0.001

Statistical Significance

p<0.05

Digital Object Identifier (DOI)

10.1186/s12903-024-04273-y

Want to read the original?

Access the complete publication on the publisher's website

View Original Publication