Effect of argon plasma and dentin rehydration on bond strength of dental adhesives to etched dentin
2024

Effect of Argon Plasma and Dentin Rehydration on Dental Adhesives

Sample size: 63 publication 10 minutes Evidence: moderate

Author Information

Author(s): Daniela Bandeira dos Santos, Vitaliano Gomes Neto, Amanda Endres Willers, Carolina Bosso André, Marcelo Giannini

Primary Institution: University of Campinas, Brazil

Hypothesis

Does dentin rehydration with water after NAPP application increase the bond strength to etched dentin, regardless of the type of adhesive?

Conclusion

Rehydration after plasma application helps maintain bond strength of dental adhesives to dentin over time.

Supporting Evidence

  • NAPP and REHY did not increase bond strength for GBU and PBU.
  • Bond strength of SBM reduced significantly after one year without NAPP treatment.
  • PBU showed the highest bond strength when applied after rehydration.

Takeaway

This study looked at how using argon plasma and water affects how well dental glue sticks to teeth. It found that adding water after using plasma helps keep the glue strong.

Methodology

The study tested three dental adhesives on human molars using bond strength tests after different treatments: control, NAPP application, and rehydration.

Potential Biases

Potential bias in sample selection and adhesive types used.

Limitations

The study was limited to specific types of adhesives and did not explore all possible variables affecting bond strength.

Participant Demographics

Human third molars were used for the study.

Statistical Information

P-Value

p<0.0001

Statistical Significance

p<0.05