Bubble-Free and Stable Potassium Metal Batteries
Author Information
Author(s): Shi Guokai, Xie Junpeng, Li Zhibin, Sun Peng, Yin Ying, Pan Likun, Hui Kwun Nam, Mai Wenjie, Li Jinliang
Primary Institution: Siyuan Laboratory, Guangdong Provincial Engineering Technology Research Center of Vacuum Coating Technologies and New Energy Materials, College of Physics & Optoelectronic Engineering, Department of Physics, Jinan University
Hypothesis
Can a bismuth oxide-modified copper host effectively suppress gas evolution in potassium metal batteries?
Conclusion
The study demonstrates that the Bi2O3 modification layer significantly reduces gas evolution and enhances the stability of potassium metal batteries.
Supporting Evidence
- The Bi2O3 layer enhances K nucleation due to its strong potassiophilicity.
- The resultant solid electrolyte interface effectively mitigates side reactions and gas generation.
- The Cu@BO@K host achieved a nucleation overpotential as low as 40 mV.
- The stability of the Cu@BO@K cell lasted for 1900 hours.
- The average Coulombic efficiency was 99.2% in the Cu@BO@K‖Cu cell.
Takeaway
This research shows how a special coating on copper can help potassium batteries work better without making gas bubbles.
Methodology
The study utilized electrochemical deposition followed by oxidation to create a bismuth oxide layer on copper, which was then tested in potassium metal batteries.
Digital Object Identifier (DOI)
Want to read the original?
Access the complete publication on the publisher's website